Compare the Impact of Degree of Conversion on Microhardness of commercially available Hybrid Dental Composites

Authors

  • Saadia Omer Department of Dental Materials, Rashid Latif Dental College, Lahore, Pakistan
  • Aiman Khan Department of Dental Materials, Khyber College of Dentistry, Peshawar, Pakistan
  • Munazzah Ejaz Department of Dental Materials, Sardar Begum Dental College, Peshawar, Pakistan
  • Muhammad Zeeshan Department of Dental Materials, Faryal Dental College, Lahore, Pakistan

DOI:

https://doi.org/10.52442/jrcd.v4i2.84

Abstract

Objective: To compare influence of degree of conversion on microhardness of nano-hybrid composites
Methodology: Two nano-hybrid composites i.e., Tetaric N Ceram by Ivoclar Vivadent, AG, Liechtenstein and Nexcomp by Meta Biomed, Korea, were chosen, and degree of conversion and hardness was calculated. T-test was used to statistically analyse the data.
Results: The degree of conversion and hardness of tartaric N Ceram was more as compared to Nexcomp and there was statistical difference between them.
Conclusion: Although the values of Nexcomp are in a lower than acceptable range, it can be used for restorative purposes.
Keywords: Composites, hardness, Degree of conversion